Bayanin Samfura

soft-magnetic-alloy-foil

Soft Magnetic Alloy : shine nau'in haɗin gwal tare da haɓaka mai ƙarfi da ƙananan iko a cikin yanayin magnetic mai rauni. Ana amfani da wannan nau'in gami a masana'antar lantarki na rediyo, kayan aikin daidaito, sarrafa nesa da tsarin sarrafa atomatik. Tare, yawanci ana amfani dashi ta fuskoki biyu: jujjuyawar kuzari da sarrafa bayanai. Abu ne mai mahimmanci a cikin tattalin arzikin ƙasa.

 Fe-Ni Magnetic Alloy Mai Laushi                                                                                                                                                                             

Darasi: 1J50 (Permalloy), 1J79 (Mumetal, HY-MU80), 1J85 (Supermalloy), 1J46

Daidaitacce: GBn 198-1988
Aikace-aikace: Mafi yawa daga ƙananan ƙananan wuta, bugun jini, mai ba da haske, masu sauyawa, masu amfani da maganadisu, haɗuwa da wutan lantarki, shaƙewa waɗanda ake amfani da su don rauni ko matsakaiciyar magnetic filayen Gudun zobe mai mahimmanci da garkuwar maganadisu.

 

Tsara 

Darasi 

Abinda ke ciki 

Makamantan Grade Na Duniya 

IEC

Rasha

Amurka

Birtaniya

High farko permeability na taushi Magnetic gami 

1J79

Ni79Mo4

E11c

79НМ

Permalloy 80 HY-MU80

Mumetal

1J85

Ni80Mo5

E11c

79НМА

Supermalloy 

-

High magnetic watsin mafi girma jikewa Magnetic juyi yawa m magnetic gami 

1J46

Ni46

E11e

46Н

45-Tsallake-Tsallake

 

1J50

Ni50

E11a

50Н

Hy-Ra49
Kamfanoni

Radiometal

  Chemistry na Fe-Ni Soft Magnetic Alloy  

Darasi

Haɗin Chemical (%)

 

C

P

S

Mn

Si

Ni

Mo

Cu

Fe

1J46

0.03

.00.02

.00.02

0.6-1.1

0.15-0.30

45-46.5

-

0.2

Bal

1J50

0.03

.00.02

.00.02

0.3-0.6

0.15-0.30

49-50.5

-

0.2

Bal

1J79

0.03

.00.02

.00.02

0.6-1.1

0.30-0.50

78.5 -81.5

3.8- 4.1

0.2

Bal

1J85

.00.03

.00.02

.00.02

0.3-0.6

0.15- 0.30

79- 81

4.8- 5.2

0.2

Bal

 Kayan Injin: 

Darasi

Resisitivity
(μΩ • m)

Desinty (g / cm3)

Matsayin Curie

Brinellhardness
HBS

TbTensile
.Arfi
MPa

Y Karfin Garkuwa
MPa

Tsawaita
(%) δ

Un-annealed

1J46

0.45

8.2

400

170

130

735

 

735

 

3

 

1J50

0.45

8.2

500

170

130

785

450

685

150

3

37

1J79

0.55

8.6

450

210

120

1030

560

980

150

3

50

1J85

0.56

8.75

400

-

-

-

-

-

-

-

-

 High jikewa magnetic shigar da taushi magnetic gami                                                                                                                

Darasi: 1J22 (Hiperco 50)

Daidaitacce: GB / T15002-94
Aikace-aikace: Shugaban wutar lantarki, muryar lasifikan waya, diaphragm, injin rotor.

Rasha Amurka Birtaniya Faransa Janpane
50KΦ Supermendur
Hiperco 50
Permendur AFK502 SME SMEV

Magungunan Chemical:

C Mn Si P S Cu Ni Co V Fe
MAX
0.025 0.15 0.15 0.015 0.010 0.15 0.25 47.5-49.5 1.75-2.10 BAL

Kayan Injin:

Denstiy
Kg / m3
g / cm3
Resisitivity
• mm• cm
Curie Poin Magnetic coefficient 10-6 Jikewa Magnetic T) (KG Na'urar roba
GPa / psi
Conarfin zafi
W / m · K/ cm · s ℃
8 120 8.12 40040 940 60 2.3823.8 207x103 29.80.0712

Coefficient na Linear Fadada/(10-6/ ° C)

20-100 ℃ 20-200 ℃ 20-300 ℃ 20-400 ℃ 20-500 ℃ 20-600 ℃ 20-700 ℃ 20-800 ℃
9.2 9.5 9.8 10.1 10.4 10.5 10.8 11.3

Ayyukan Magnetic

Sigogi Girma /mm / a Mafi qarancin jujjuyawar ruwa / don tsananin ƙarfin maganadisu mai zuwaTKG
800 A / m
10A
1.6KA / m
20da
4KA / m
50Oe
8KA / m
100A
Tsiri   2.0020.0 2.121.0 2.2022.0 2.2522.5
Bar 12.7-25.40.500-1 1.6016.0 1.8018.0 2.0020.0 2.1521.5
Sanda > 12.71 1.5015.0 1.7517.5 1.9519.5 2.1521.5